Figure 11: 3mm 두께 1.4301 스테인리스강에 LASGON®C1을 사용한 산업적 적용 사례(200W, 1m/min)를 보여줍니다. 6. 참고문헌 Wada and Pehlke. According to Wada and Pehlke, the hot metal can absorb between 440 and 500 µg nitrogen per gram iron (Fig. 3).