1.0% Sc. Figure 1. Microstructure of the heat-treated alloy ML10, magnification 500: (a) without Sc; (b) 0.05% Sc; (c) 1.0% Sc.

1.0% Sc.
Figure 1. Microstructure of the heat-treated alloy ML10, magnification 500: (a) without Sc; (b) 0.05%
Sc; (c) 1.0% Sc.