Fig. 10 SEM observations of the initiation site on the fracture surface in cast iron specimens containing a foundry defect: big grain of graphite (800×150 μm)

Fig. 10 SEM observations of the initiation site on the fracture surface
in cast iron specimens containing a foundry defect: big grain of
graphite (800×150 μm)