Fig. 3. Nylon 11 impact sequence onto a preheated substrate

Fig. 3. Nylon 11 impact sequence onto a preheated
substrate, (I) partially melted particle before impact,
(II) “fried-egg” shaped splat, (III) post-deposition flow
of a fully molten droplet, (IV) droplet shrinkage during
cooling.